These bases and hoods have been developed to address the problem of corrosion cracking between different replacement parts, such as levers, die-cast components, and fasteners, caused by electrochemical reactions. Tests have demonstrated that these bases and hoods withstand salt spray, in accordance with IEC 60512-11-6:2002, for more than 500 hours.
These new bases and hoods are specifically designed for applications where salt spray poses a challenge to components, such as wind turbines, railways, cranes, and other outdoor applications.